"M. P. Edison" <[log in to unmask]>
Reply To:
Date:
Thu, 31 Oct 2002 12:06:03 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (27 lines)
> >
> > But if it has a Tg of say, 55 F, it might seem awfully hard on a
> > chilly late October day.
>
> My site inspection was this past summer. It was hot. The coating was
> hard.
>
> Sign me, dan hard like my head becker
>
If the coating is really very hard, then the 150% elongation reported
could be suspect. I don't recall seeing any hardness data, however.

Edison Coatings, Inc.
M. P. Edison
President
3 Northwest Drive
Plainville, CT 06062  USA
Phone: (860)747-2220
Fax: (860)747-2280
email: [log in to unmask]
Internet: www.edisoncoatings.com

--