> > But if it has a Tg of say, 55 F, it might seem awfully hard on a
> > chilly late October day.
>
> My site inspection was this past summer. It was hot. The coating was
> hard.
>
> Sign me, dan hard like my head becker
>
If the coating is really very hard, then the 150% elongation reported
could be suspect. I don't recall seeing any hardness data, however.
Edison Coatings, Inc.
M. P. Edison