If one were concerned with bond, say for a very low Initial Rate of
Absorption (such as 5.5 grams/minute/30 sq. inches when the ASTM recommended
range is 5-25), could you control or slow the cure to improve bond strength
by increasing the lime in a cement/lime mortar? Would you want to?